Comparative Real-Time Characterization Of Frother Bubble Thin Films

Society for Mining, Metallurgy & Exploration
S. Gélinas J. A. Finch M. Gouet-Kaplan
Organization:
Society for Mining, Metallurgy & Exploration
Pages:
4
File Size:
390 KB
Publication Date:
Jan 1, 2006

Abstract

Methylisobutyl carbinol (MIBC) and methoxy polypropylene glycol (Dowfroth 250) bubble thin films were characterized by composition and thickness determinations, using FT-IR spectroscopy and UV-Visible spectrophotometry, respectively. The infrared investigation indicates that the role of frother molecules in creating bubble thin films is based on their effectiveness in inducing H-bonding reorganization of the surrounding free water molecules into a coherent network. From UV-Visible interference patterns, it is found that MIBC forms films with a measured critical end thickness of less than 160 nm, compared to 612 ± 30 nm for Dowfroth 250. The observed values of the free water layer thickness are comparable at 5.65 ± 0.28 µm for MIBC and 6.75 ± 0.34 µm for Dowfroth 250. A higher stability of an MIBC bubble over a Dowfroth 250 bubble is related to the different polarization and orientation of the molecules sustaining the boundary surface water network. The findings are used to explain the different action and associated froth characteristics of the two common industrial frothing agents.
Citation

APA: S. Gélinas J. A. Finch M. Gouet-Kaplan  (2006)  Comparative Real-Time Characterization Of Frother Bubble Thin Films

MLA: S. Gélinas J. A. Finch M. Gouet-Kaplan Comparative Real-Time Characterization Of Frother Bubble Thin Films. Society for Mining, Metallurgy & Exploration, 2006.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account