Dewatering and Water Recycling Experiments on Bauxite Flotation Tailings

International Mineral Processing Congress
Yuhua Wang Dongfang Lu Yanqing Jiang Huilan Yang
Organization:
International Mineral Processing Congress
Pages:
17
File Size:
596 KB
Publication Date:
Jan 1, 2018

Abstract

"Generally, the concentration of bauxite flotation tailings is around 10%, a large amount of water in tailings needed to be recycled in the flotation process. Sedimentation and dewatering properties of tailings were investigated under different conditions. Surface high negative charges on mineral particles are the key factor to destroy the settlement of tailings when the pulp pH is around 8.9. Hence, the modification of pulp pH around 7 is necessary to the diminution of the repulsive force between mineral particles and then the acceleration of sedimentation of tailings. Anionic polyacrylamine with molecular weight of 14 million is the best flocculant for the settlement of tailings in all tested polyacrylamines. P-toluene sulfonic acid shows better properties than hydrochloric acid for pulp pH adjustment when anionic polyacrylamine with molecular weight of 14 million is used as flocculant. Although the flotation of diaspore is depressed in the presence of polyacrylamine using sodium oleate as collector, but the recycling water traded by the combination of ployacrylamine and p-touenesulfonic acid does not show the depression effects on the flotation of bauxite ore. The lower residual content of polyacrylamine in recycling water treated by the combination of ployacrylamine and p-touene sulfonic acid plays an important role. INTRODUCTION Generally, the waste water generated from mineral processing plant is usually treated by sedimentation, oxidization, electrodialysis, ions exchange, active carbon adsorption and flotation technology, and the treated water is also used again in the industrial process. Flotation was adopted widely to improve the quality of bauxite from low grade diasporic bauxite in China. For flotation, the grinding fineness of bauxite is over 90% -0.074 mm, sodium carbonate and sodium hexametaphosphate were used as regulators, so the tailings pulp is very difficult to settle and be dewatered (Y. Wang et al., 2004; Y. H. Wang et al., 2007; Wang Yu-hua et al., 2008; Wang Yuhua et al., 2011). The water recycling of bauxite tailings are becoming the highlight for the industrial application of the flotation process for bauxite ore. Researchers in China shift their attentions onto this topic."
Citation

APA: Yuhua Wang Dongfang Lu Yanqing Jiang Huilan Yang  (2018)  Dewatering and Water Recycling Experiments on Bauxite Flotation Tailings

MLA: Yuhua Wang Dongfang Lu Yanqing Jiang Huilan Yang Dewatering and Water Recycling Experiments on Bauxite Flotation Tailings. International Mineral Processing Congress, 2018.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account