Abstract
A novel process for the preparation of a-Al2O3 from secondary aluminum dross was studied. Factors including alkali dross ratio, salt dross ratio, smelting temperature, smelting time, leaching temperature, leaching time, and the solid-liquid ratio, which possibly influence the transfer of Al into water were studied, and the feasibility of using seed precipitation as a treatment technology of the leachate was discussed. The optimum condition of the process was determined as: alkali dross ratio 1.3, salt dross ratio 0.7, smelting temperature 500°C, smelting time 60min, leaching temperature 60°C, leaching time 30min, solid-liquid ratio 1:4. The results show that using the seed precipitation method, the leaching of aluminum reaches 92.71%, demonstrating the technique as a feasible and effective treatment technology of the leachate.
Citation
APA: (2011) High-Effective Process for the Preparation of A-Al203 Using Secondary Aluminum Dross as Raw Material
MLA: High-Effective Process for the Preparation of A-Al203 Using Secondary Aluminum Dross as Raw Material. Canadian Institute of Mining, Metallurgy and Petroleum, 2011.