Interactions Of Two-Liquid CaO-MgO-FetO-P2O5 Slag With MgO Refractories

The Southern African Institute of Mining and Metallurgy
T. Tamura
Organization:
The Southern African Institute of Mining and Metallurgy
Pages:
4
File Size:
624 KB
Publication Date:
Jan 1, 2004

Abstract

It is known that the CaO-FetO-P2O5slag system has a wide liquid miscibility gap at steelmaking temperatures and this two-liquid slag phase has many advantages such as high activities of both FetO and CaO and high amount of P2O5. The phosphorus distribution ratio between the two-liquid slag and molten steel was confirmed to be higher than that between CaOsat.-FetO-P2O5slag and molten steel. The two-liquid slag may be useful for dephosphorization of molten steel and reduction of slag volume. Furthermore, the phase equilibrium of two-liquid CaO-FetO-P2O5slagsaturated with MgO was measured to determine the applicability of the two-liquid slag to dephosphorization in steelmaking process. Keywords: slag, refractories, solid solution, two-liquid phase, dephosphorization, steelmaking, phase equilibrium.
Citation

APA: T. Tamura  (2004)  Interactions Of Two-Liquid CaO-MgO-FetO-P2O5 Slag With MgO Refractories

MLA: T. Tamura Interactions Of Two-Liquid CaO-MgO-FetO-P2O5 Slag With MgO Refractories. The Southern African Institute of Mining and Metallurgy, 2004.