Abstract
Ammonia - ammonium sulfate solutions were sparged in a glass reactor with a SO2/O2 gas mixture (2% SO2 and 98% O2) to leach copper from pure chalcopyrite and chalcopyrite concentrate. The SO2/O2 mixture produces higher and faster extractions than O2 by itself. The effect of temperature, particle size and free ammonia concentration was investigated. The fastest and highest recoveries were obtained at 80 oC from a chalcopyrite concentrate with a d80equal to 13 m, with about 83 gpl free ammonia, an average pH equal to 8.75 and a stirring speed of 500 rpm. The extraction process was controlled by diffusion through a product layer, according to the shrinking core model, with an activation energy of 41 kJ/mole.
Citation
APA:
(2003) Leaching of Chalcopyrite in Ammoniacal Solutions Sparged with a SO2/O2 Gas MixtureMLA: Leaching of Chalcopyrite in Ammoniacal Solutions Sparged with a SO2/O2 Gas Mixture. The Minerals, Metals and Materials Society, 2003.