Preparation Of Al-Ti Master Alloys By Aluminothermic Reduction Of Tio₂ In Cryolite Melts At 960°C

The Minerals, Metals and Materials Society
Aimin Liu Kaiyu Xie Liangxing Li Zhongning Shi Xianwei Hu Junli Xu Bingliang Gao Zhaowen Wang
Organization:
The Minerals, Metals and Materials Society
Pages:
8
File Size:
587 KB
Publication Date:
Jan 1, 2015

Abstract

Al-Ti master alloys were prepared by aluminothermic reduction between the dissolved titanium dioxide and aluminum in cryolite melts at 960oC. The kinetic analysis by differential scanning calorimetry indicated that the apparent activation energy of the reaction of reducing titanium dioxide by aluminium is 22.3 kJ/mol, and the reaction order is 0.5. The products were analyzed by means of X-ray diffraction, X-ray fluorescence, scanning electron microscopy and energy dispersive spectrometer. Results from X-ray diffraction showed that the phase compositions of produced alloys are Al and Al3Ti. In addition, Al-Ti master alloys containing 2-6 mass% Ti were formed at different reduction time of 2-5h in aluminothermic reduction experiment.
Citation

APA: Aimin Liu Kaiyu Xie Liangxing Li Zhongning Shi Xianwei Hu Junli Xu Bingliang Gao Zhaowen Wang  (2015)  Preparation Of Al-Ti Master Alloys By Aluminothermic Reduction Of Tio₂ In Cryolite Melts At 960°C

MLA: Aimin Liu Kaiyu Xie Liangxing Li Zhongning Shi Xianwei Hu Junli Xu Bingliang Gao Zhaowen Wang Preparation Of Al-Ti Master Alloys By Aluminothermic Reduction Of Tio₂ In Cryolite Melts At 960°C. The Minerals, Metals and Materials Society, 2015.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account