Abstract

Leaching studies of magnesite obtained from Tamilnadu Magnesite Limited, Salem, have been carried out using hydrochloric acid leaching and percentage of magnesium chloride recovered was estimated. The variables considered in this study were the following: duration of leaching, volume percentage of hydrochloric acid, temperature, and pulp density. Percentage recovery of magnesium chloride increased with duration of the leaching, volume % of concentrated hydrochloric acid, and temperature. Percentage recovery of magnesium chloride decreased with increase of pulp density. The optimum conditions found to be pulp density (10%), hydrochloric acid concentration (30%), duration of leaching (2 h), and temperature (348.15 K). Iron was removed by treating the leach liquor with hydrogen peroxide and by raising the pH to 3.5–4. The purified leach liquor was subjected to spray drying for producing high pure magnesium chloride.
Citation

APA: Venkata Swamy Nalajala Naga Jyothi Kothamasu Tondepu Subbaiah Ramesh Naidu Mandapati Ch. R. V. S. Nagesh  (2022)  Preparation of Magnesium Chloride from Magnesite Dust Using Hydrochloric Acid Leaching and Spray Drying

MLA: Venkata Swamy Nalajala Naga Jyothi Kothamasu Tondepu Subbaiah Ramesh Naidu Mandapati Ch. R. V. S. Nagesh Preparation of Magnesium Chloride from Magnesite Dust Using Hydrochloric Acid Leaching and Spray Drying. Society for Mining, Metallurgy & Exploration, 2022.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account