The research and development of new, more selective collectors in order to improve flotation efficiency represent one of the main priorities in the development of innovative technologies pertaining to flotation separation of various substances and minerals. The use of collectors’ mixtures is considered as the universal instrument for ensuring necessary proportion of chemically and physically sorbed collecting reagents in every individual case. Currently hard-dressed, refractory ores and man-made raw materials, which are characterized by low content of valuable components, fine dissemination of mineral assemblages and similar technological properties of constituent minerals, are widely involved in the recycling processes. The possibility of processing tailings, which are left after flotation beneficiation, has been considered in the case study of tailings of the Zhezkazgan beneficiation plant and the Tishinsk copper ore deposit with utilization of the modified multifunctional flotation reagents. Modified poly-functional collector is the mixture of composite Aerofloat, TC-1000 and butyl xanthate. Reactants ratio is 1:1:3. The advantage of the suggested flotation reagents is that they are composed of two polar groups and have a long hydrocarbon radical. This structure, being in the water during flotation process, plays a dual role: first, as a collector adsorbing on the mineral surface it produces metal complexes with polar groups in the form of bridges; second, apolar radicals flocculate valuable slimed components, thereby intensifying flotation process. It has been shown that flotation of Zhezkazgan tailings with utilization of the lesser modified reagent amount compared to butyl xanthate has enabled to produce crude copper concentrate with 13.0 % copper grade and 80.22 %recovery. Compared to the baseline technology, copper content of crude concentrate has been increased by 5.1 % and the recovery by 31.4 %. It is shown that tailings flotation of the Tishinsky field by applying modified collector allows for increase of the of useful components extraction in a collective concentrate with: copper 9.63 %, lead for 8.41%, zinc 9.2 %, iron 2.73 %, gold 3.57 %.
Citation

APA: N. K. Tussupbayev L. V. Semushkina D. K. Turysbekov S. M. Narbekova A. M. Muhamedilova  (2018)  Processing Of Flotation Tailings from Benefication by Using Modified Flotation Reagents

MLA: N. K. Tussupbayev L. V. Semushkina D. K. Turysbekov S. M. Narbekova A. M. Muhamedilova Processing Of Flotation Tailings from Benefication by Using Modified Flotation Reagents. International Mineral Processing Congress, 2018.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account