Abstract
"INTRIDUCTION At present, more and more metallized raw materials with a metallization degree of not less than 80% are used in the smelting of steel. The main quantity of this raw material is produced in furnaces of mine type. Advantages of this type of raw materials for metallurgical processing are low levels of harmful and slag-forming impurities and a high content of metallic iron. At the same time, the cost of smelting raw materials and obtaining high-quality steels are reduced. In addition to the undoubted merits of metallized raw materials, there are high requirements for the quality of iron concentrates, which are the starting material for metallization: the mass fraction of acidic oxides should not exceed 3%; The mass fraction of iron should not be less than 69%, mass fractions of harmful impurities (phosphorus, arsenic, sulfur, copper, etc.) should not exceed 0.02%. These requirements are dictated by the fact that the recovery of burned pellets is carried out by gas in a solid phase. In this case, the empty rock and harmful impurities from the metal are not separated and sent to the steelmaking unit, increasing the heat consumption for heating and worsening the quality of the steel. The combined production of high-quality concentrate and metallized raw materials requires a large capital outlay from the enterprise, which in the future can be compensated for by increased profit from the sale of more expensive marketable products. At present, in the territory of Russia and the CIS countries Lebedinsky mining-and-processing integrated works is the only enterprise that carries out the entire chain of operations for the production of metallized raw materials, starting with the production of high-quality magnetite concentrate with a mass fraction of iron of 69.5% and ending with the production of a metallized product in the form of hot briquetted gland. JSC «SSGPO» is the largest iron-processing enterprise in Kazakhstan, which processes about 40 million tons of ore per year and receives 16 million tons of concentrate per year with a mass fraction of iron 66.0-66.5%. The technological scheme existing at the concentrator of JSC ""SSGPO"" includes the crushing of the feed ore to the size of 20-0 mm; dry magnetic separation operation; three reduction stages to a fineness of 90-95% kl-0.071 mm; operation of desliming, wet magnetic separation and filtration of the concentrate. Dry magnetic separation of the feed ore makes it possible to remove from the process of 19.6% of the tailings with a mass fraction of the total iron 12.5%, of magnetite 2.2%. The first reduction stage is carried out in rod mills with the volume of 40 m3 to a size of -1.6 + 0.0 mm. The first stage of wet magnetic separation is carried out in counterflow magnetic separators PBM-P-150/200L. The magnetic product of the first stage of WMS is classified in hydrocyclones; sands enter the second reduction stage into central discharge ball mill 3600 × 5000. Runoff of mills enter on the second enrichment stage in counterflow magnetic separators PBM-P-150/200L. The magnetic product enters the classification of the second stage, forming a closed cycle. Mass fraction of the class -0.071 + 0 mm in classifications runoff of the second stage is 70-75%. The second stage classifications runoff is transported toWMS-III operation in semi-counter separators PBM-PP-120/300. The magnetic product of the third stage enters the classification of the third stage. Granular residue are transported to the reduction of the third stage into central discharge ball mill 3600 × 5000. The mill runoff enters the third stage of classification, forming a closed cycle. Classifications runoff of the third stage enters on deslimation. Deslimed product is sent for fine screening to the crasher «Derrick» 2SG48-60W-5STK with a cell size of 0.1 mm. Top size of crasher is sent to regrinding. Undersize with a mass fraction of the class -0.071 + 0 mm 90-95% is fed to the wet magnetic separation of WMS-"
Citation
APA:
(2018) Production of High-Quality Magnetite Concentrate from Scarn Ore by JSC "SSGPO"MLA: Production of High-Quality Magnetite Concentrate from Scarn Ore by JSC "SSGPO". International Mineral Processing Congress, 2018.