RI 9415 - Cause of Floor Self-Heatings in an Underground Coal Mine (f50c25d5-acc4-494c-901f-26455f6e764b)

The National Institute for Occupational Safety and Health (NIOSH)
Y. Miron
Organization:
The National Institute for Occupational Safety and Health (NIOSH)
Pages:
30
File Size:
2731 KB
Publication Date:
Jan 1, 2010

Abstract

'This report presents a U.S. Bureau of Mines study to identify the causes of self-heating events beneath the floor of a deep underground coal mine. Mine samples from both heated and unheated areas were examined by various techniques, including visual, microscopic, thermal, chemical, and instrumental tests. The combined results led to the conclusion that pyrite (FeS2) oxidation was the prime cause of the beatings. However, adiabatic oven tests of selected samples did not indicate the effect of the pyrite on the self-heating process, probably because of the experimental conditions. A fast, simple procedure to assess the concentration of pyrite in the mine samples was developed, g the reactivity of the sample with an aqueous solution of hydrogen peroxide (H2O2).
Citation

APA: Y. Miron  (2010)  RI 9415 - Cause of Floor Self-Heatings in an Underground Coal Mine (f50c25d5-acc4-494c-901f-26455f6e764b)

MLA: Y. Miron RI 9415 - Cause of Floor Self-Heatings in an Underground Coal Mine (f50c25d5-acc4-494c-901f-26455f6e764b). The National Institute for Occupational Safety and Health (NIOSH), 2010.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account