Abstract
In order to recover Ti resource from titanium bearing blast furnace slag, a new technology to separate perovskite phase from CaO-TiO2-SiO2-Al2O3-MgO system by supergravity is researched. In the condition of gravity coefficient of 750g, treatment temperature of 1305°C and time of 20min, the significant layers appear in samples which are obtained by means of centrifugal treatment. Along the direction of the supergravity, the volume fraction of perovskite phase increases gradually, and the equivalent diameters of perovskite phase crystals increases with the area approaching to the bottom of the sample. It is indicated that TiO2 is enriched in the bottom of sample as concentrate with a recovery ratio of 74.05% by supergravity treatment.
Citation
APA:
(2014) Separation of Perovskite Phase from Cao-Tio2-Sio2-Al2O3- MgO System by SupergravityMLA: Separation of Perovskite Phase from Cao-Tio2-Sio2-Al2O3- MgO System by Supergravity. The Minerals, Metals and Materials Society, 2014.