Stress-Corrosion Testing of Copper-Base Alloys

The American Institute of Mining, Metallurgical, and Petroleum Engineers
C. L. Bulow
Organization:
The American Institute of Mining, Metallurgical, and Petroleum Engineers
Pages:
25
File Size:
2463 KB
Publication Date:
Jan 1, 1945

Abstract

In this discussion of stress-corrosion cracking of widely used copper-base alloys, no attempt has been made to prepare an extensive review or bibliography since this has been quite ably covered by other investigators. An excellent bibliography was published by H. P. croft(1)2 in connection with his studies of stress-corrosion cracking in mercurous nitrate solutions and his analyses of the magnitude and distribution of stresses in brass parts. We are reporting on a few of the results which have been obtained to date in connection with an ammonia vapor test and an alternate immersion test. These are accelerated corrosion tests for determining the susceptibility of materials to failure from season or stress-corrosion cracking due to the presence of moist ammonia and oxygen so prevalent in nature. Our experiences with the ammonia test seem to indicate that it is a more searching test, than the mercurous nitrate test.
Citation

APA: C. L. Bulow  (1945)  Stress-Corrosion Testing of Copper-Base Alloys

MLA: C. L. Bulow Stress-Corrosion Testing of Copper-Base Alloys. The American Institute of Mining, Metallurgical, and Petroleum Engineers, 1945.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account