Stress Intensity Factors of Chevron-Notched Semi-circular Specimen

The Australasian Institute of Mining and Metallurgy
Organization:
The Australasian Institute of Mining and Metallurgy
Pages:
3
File Size:
478 KB
Publication Date:
Jan 1, 1998

Abstract

A three-dimensional finite element analysis is used to determine the stress intensity factors associated with the chevron-notched semi-circular bend test specimen. The stress intensity factor calibration is done over a range of crack lengths a