Viscosity Property Of Gold-Antimony Smelting Slags By Blast Furnace

The Minerals, Metals and Materials Society
Yongbin Yang Qiang Zhong Tao Jiang Qian Li Bin Xu
Organization:
The Minerals, Metals and Materials Society
Pages:
8
File Size:
480 KB
Publication Date:
Jan 1, 2015

Abstract

Viscosity of slag determines the production efficiency, energy consumption and distribution of elements between metal and slag, which is very important for pyrometallurgy. Slag of goldantimony ore blast furnace smelting has seldom been studied. In this paper, the viscosities of gold-antimony ore smelting slags of different composition have been studied by the rotating cylinder method. The results showed that, for a slag of 38.95% SiO2, 16.17% CaO, 25.97% FeO, 10.25% Al2O3, 5.17% MgO, the viscosity can be decreased by reducing 3.24%-8.5% SiO2 or increasing 3.31%-9.56% CaO content. Complex SixOy z- from SiO2 acts as the main cause for the high viscosity in a slag of high SiO2. The increasing of CaO causes the decreasing of the amount of SixOy z- and the O2- dissociated from CaO breaks the complex SixOy z-, which can decrease the viscosity. Viscosity of different composition slag in the appropriate range temperature can be calculated from the Arrhenius equation.
Citation

APA: Yongbin Yang Qiang Zhong Tao Jiang Qian Li Bin Xu  (2015)  Viscosity Property Of Gold-Antimony Smelting Slags By Blast Furnace

MLA: Yongbin Yang Qiang Zhong Tao Jiang Qian Li Bin Xu Viscosity Property Of Gold-Antimony Smelting Slags By Blast Furnace. The Minerals, Metals and Materials Society, 2015.

Export
Purchase this Article for $25.00

Create a Guest account to purchase this file
- or -
Log in to your existing Guest account