Co-Cr-Mo Alloys Production by Self Propagating High Temperature SynthesisBy Onuralp Yiicel, Ozlem Okur, Murat Alkan
"In this study, Co-Cr-Mo alloys were produced using a mixture of Co304, Cr203 and Mo03 powders with Al powders by a Self-propagating high temperature synthesis process. SHS is a process of material sy
Jan 1, 2013
-
Shape Memory Characteristics Of Rapidly Solidified Ti-37.8Cu-18.7Ni Alloy RibbonsBy Alana Pereira Ramos, Walman Benicio de Castro
Amorphization and martensitic transformation (Ms) characteristics of Ti–Ni-Cu alloy ribbons prepared by melt spinning were investigated by means of differential scanning calorimetry and X-ray diffract
Jan 1, 2015
-
Microstructural Defects-Strength Relationship of Silicon Nitride CeramicsBy Keizo Uematsu, Satoshi Tanaka, Nozomu Uchida, Ronne Hendrajaya
"The influence of microstructural defects on strength in Si3N4 is reviewed. The presence of cracks, pores and inclusions greatly affects the strength of Si3N4. The micron order crack size and distribu
Jan 1, 2000
-
Ultra Fine Particle DepositionBy Suk J. Im, I. S. Min, Daesoo Kim
UFP are defined by atoms or their clusters having diameter in the range of l0Å-0.l.um. Due to a ratio of very large surface area to volume, they have peculiar properties such as extra high surface ene
Jan 1, 1988
-
Morphological study of rolling contact fatigue of nitrogenated carbon coated steels (Poster Paper)By Byung-Young Choi
Nitrogenated carbon films were deposited on the high-frequency induction hardened steels by ion beam assisted deposition. X-ray photoeleetron. spectroscopy and scanning electron microscopy were used t
Jan 1, 2000
-
Mechanical Properties of Friction Stir Welded Inconel 600/SS 400 Lap JointsBy W. Y. Kim, K. H. Song, K. Nakata
"The present study was carried out to evaluate the mechanical properties of friction stir welded Inconel 600/SS 400 lap joints. In this process, friction stir welding (FSW) was performed at a tool rot
Jan 1, 2012
-
SEM Characterization Of Lignite Fly AshBy Robert J. Stevenson
The chemical variation of central North American lignite fly ash can be compared using the major and minor oxide analyses and the distribution pattern of the inter-grain chemistries of the individual
Jan 1, 1992
-
Single Stage Copper Making-Flowsheet DevelopmentBy M. Somerville
In 1989 CSIRO Minerals initiated investigations into continuous converting of copper matte into low sulphur blister in Sirosmelt type reactors. Following the successful piloting of this processing rou
Jan 1, 1999
-
Fused Salt Electrolysis Of Rare Earth MetalsBy Donald R. Sadoway
Fused salt electrolysis is used extensively in the primary extraction of metals (electrowinning), in the refining of metals (electrorefining), and in the formation of coatings (electroplating). In the
Jan 1, 1989
-
Recovery of Copper from Printed Circuit Boards Waste by BioleachingBy Jorge Alberto Soares Tenório, Denise Crocce Romano Espinosa, Luciana Harue Yamane
"The present work investigated the influence of Fe+2 initial concentrations in the bioleaching of copper from printed circuit board using Acidithiobacillus ferrooxidans-LR. Printed circuit boards were
Jan 1, 2011
-
Improvements To Taphole DesignBy Melissa L. Trapani
The removal of molten products from metallurgical furnaces is one of the most hazardous and labour intensive processes in a non-ferrous smelter. The proximity of operators to the molten metal and slag
Jan 1, 2002
-
Characterization of Grit Blasted Metallic Biomaterials by Thermoelectric Power MeasurementsBy F. G. Caballero, J. L. Gonzalez-Carrasco, S. Barrius, H. Carreon, M. Lieblich
"The grit blasting is a low-cost technique successfully used to enhance mechanical fixation of the implants through increasing their roughness. As a result of the severe plastic surface deformation, i
Jan 1, 2012
-
Recent Operational Improvements At Saganoseki SmelterBy Yoshiaki Suzuki
In 1996, Saganoseki smelter & refinery successfully shifted to a single flash smelting furnace operation and increased the copper production capacity to 450,000mtpy in 1998. As the next step, Saganose
Jan 1, 2006
-
Leaching Of Copper Concentrate By A Chemical Catalytic Oxidation MethodBy Burkhard Seeger et al.
The oxidation of copper sulfides can be highly accelerated in the presence of nitrous gases (NOx) as reaction catalysts. Sulfur and sulfate are simultaneously produced in this highly exothermic reacti
Jan 1, 1999
-
Numerical Simulation of Erosion Using Computational Fluid DynamicsBy H. Singh, Anupam Agrawal, H. S. Grewal
"Erosion in industrial appliances causes huge loss of valuable resources especially when solid particles are present in the working medium. A number of erosion models that are available in the literat
Jan 1, 2012
-
Pressure Leaching Of White Metal As An Alternative To ConversionBy María Cristina Ruiz
In the processing of copper concentrates by the conventional smelting-converting technology, complying with the increasingly severity of environmental legislation in some countries has become difficul
Jan 1, 2006
-
Recovery Of Metals From Steelmaking Dust By Selective Chlorination ? Evaporation ProcessBy Hiroyuki Matsuura
Treatment of electric arc furnace (EAF) dusts has become an important issue from the viewpoint of the environmental protection and recycling of variable resources because these dusts contain considera
Jan 1, 2006
-
Cellhouse VentilationBy J. de Visser, J. A. Davis
Since the mid 1970's, development of zinc electrowinning (EW) facilities has out-paced its counterparts in the copper and nickel electrowinning industries in the design of efficient, compact, and auto
Jan 1, 2000
-
Characterization of Open-Pored Metals Using Image ProcessingBy Björn Hinzel, Joachim Rösler
"The most important characteristic of open-pored metals is porosity, since it enables all of their functional applications as filters or sound absorbers. Due to the notch effect of the pores, mechanic
Jan 1, 2012
-
Effervescence During Desulfurization Of Copper MeltsBy R. Harris
Blister copper melts of 800 g to 1000 g containing less than 1 wt % S and up to 3 wt % Ni were desulfurized at 1523 K in air or by a pure oxygen jet blown at 75,500 and 1000 cm3/min, from 1 cm above t
Jan 1, 1999